Maila zk. | Itxura | Biguntze-puntua /℃ | Konbergentzia-tasa /s | Pelletaren emaria /mm (125 ℃) | Fenol askea/% | Ezaugarria |
DR-103 | Partikula horia ahulak uniformeak | 90 -93 | 28-35 | ≥70 | ≤3,5 | Polimerizazio-tasa/eredu eta nukleo ona |
DR-106C | Partikula horia ahulak uniformeak | 95 -98 | 20 -27 | ≥45 | ≤3,0 | Polimerizazio-tasa ona Azalaren aurkakoa |
DR-1387 | Partikula horia ahulak uniformeak | 85 -89 | 80-120 | ≥120 | ≤1,0 | Indar handia |
DR-1387S | Partikula horia ahulak uniformeak | 87 -89 | 60 -85 | ≥120 | ≤1,0 | Indar handia |
DR-1388 | Partikula horia ahulak uniformeak | 90 -94 | 80 - 1 10 | ≥90 | ≤0,5 | Tarteko indarra Ingurumena errespetatzen duena |
DR-1391 | Azafraiaren partikula horia uniformeak | 93 -97 | 50 -70 | ≥90 | ≤1,0 | Altzairu urtua |
DR-1391Y | Partikula horia ahulak uniformeak | 94 -97 | 90-120 | ≥90 | ≤1,0 | Altzairu urtua Ingurumena errespetatzen duena |
DR-1393 | Partikula horia ahulak uniformeak | 83 -86 | 60 -85 | ≥120 | ≤2,0 | Indar ultra-altua |
DR-1396 | Azafraiaren partikula horia uniformeak | 90 -94 | 28-35 | ≥60 | ≤3,0 | Polimerizazio-tasa ona Tarteko indarra |
Paketatzea:
Paperezko plastikozko poltsa konposatua ontziratzea eta plastikozko poltsekin forratuta, 40kg/poltsa, 250kg, 500kg/ton poltsa.
Biltegiratzea:
Produktua biltegi lehor, fresko, aireztatuta eta euri-kontrako batean gorde behar da, bero-iturrietatik urrun. Biltegiratze-tenperatura 25 ℃ baino txikiagoa da eta hezetasun erlatiboa % 60tik beherakoa da. Biltegiratze epea 12 hilabetekoa da, eta iraungitakoan berriro probatu eta sailkatu ondoren produktua erabiltzen jarraitu daiteke.